Dentin bond strengths of three adhesive/composite core systems using different curing units.

Dentin bond strengths of three adhesive/composite core systems using different curing units.

Dent Mater J. 2008 Mar;27(2):187-94

Authors: Ariyoshi M, Nikaido T, Okada A, Foxton RM, Tagami J

Abstract

This study evaluated the tensile bond strengths of three adhesive/composite core materials to bovine dentin using three different curing units. Bovine dentin surfaces were ground with 600-grit SiC paper. Bonding area was demarcated with a vinyl tape (4-mm-diameter hole). Three adhesive/composite core systems–S6054 (experimental), UniFil Core, and Clearfil DC Core Automix–were used with three curing units–Curing Light XL3000 (quartz-tungsten-halogen), Hyper Lightel (high-power quartz-tungsten-halogen), and LEDemetronl (blue light-emitting diode)–according to manufacturers’ instructions. After 24 hours of storage in water at 37 degrees C, tensile bond strengths were measured at a crosshead speed of 2 mm/min. Results were statistically analyzed with one-way ANOVA and Tukey’s HSD test (p < 0.05). Highest tensile bond strength was obtained using Clearfil DC Core Automix with Hyper Lightel.

[cite source='pubmed']18540391[/cite] – indexed for MEDLINE]