Dent Mater J. 2020 Dec 3;39(6):1050-1056. doi: 10.4012/dmj.2019-331. Epub 2020 Jul 17.
ABSTRACT
This study compared the effect of experimental polymer-based desensitizers with NaF and oxalic acid (OA) for preventing root demineralization via observation using micro-CT. Bovine root dentin surfaces were treated with coating materials: no treatment; MS0(+) (MS Coat One®); MS3000(+) (MS Coat®); MS0(-); MS3000(-); MS7000(+/-); fluoride gel (NaF9000). MS; MS polymer, 0-7000; NaF concentrations, (+/-); OA. The specimens were scanned using micro-CT before and after demineralization (pH4.5, 10 h). Following this, the mean mineral loss (ML) after demineralization was calculated, and the specimens were observed under a scanning electron microscope (SEM). The ML values of MS3000(+), MS7000(-), MS7000(+) and NaF9000 were significantly lower than the other groups (p<0.05). Under an SEM, a membrane structure was observed to have formed on the dentin surface in the presence of the MS, fluoride, and OA. The experimental polymer-based desensitizer with oxalic acid and a high concentration of fluoride is effective for preventing root demineralization.
PMID:32684611 | DOI:10.4012/dmj.2019-331