Nov 24 2021

Can a New HEMA-free Two-step Self-etch Adhesive Improve Dentin Bonding Durability and Marginal Adaptation?

J Adhes Dent. 2021 Dec 3;23(6):505-512. doi: 10.3290/j.jad.b2288233.

ABSTRACT

PURPOSE: A new two-step self-etch adhesive (2-SEA) free of hydrophilic monomers was evaluated. Its microtensile bond strength (µTBS) to dentin under various aging conditions, interfacial gap formation, water sorption/solubility, and formation of an acid-base resistant zone (ABRZ) were evaluated and compared with a gold-standard 2-SEA.

MATERIALS AND METHODS: The new 2-SEA G2-Bond Universal (G2; GC) was compared to Clearfil SE Bond 2 (CSE2, Kuraray Noritake). Their µTBS to sound coronal dentin was tested after 1 week, 10,000 thermal cycles (TC), 20,000 TC, 6 months and 1 year. Failure mode was determined using scanning electron microscopy (SEM). Gap formation at the interface of 2-mm deep tapered cavities with an enamel border was observed using swept-source optical coherence tomography after 1 day, 1 week, 10,000 TC, and 20,000 TC. In addition, water sorption and solubility of the bonding agents was measured, and ABRZ formation was evaluated using SEM.

RESULTS: There was no significant difference in µTBS between G2 and CSE2 (p > 0.05), and the aging conditions had no significant effect on µTBS (p > 0.05). In all groups, cohesive failures prevailed (55%-95%). Interfacial gap formation was initially similar for both adhesives (p > 0.05), but G2 exhibited a significantly lower gap formation than CSE2 after TC (p < 0.05). The water sorption of G2 was significantly lower compared to CSE2 (p < 0.05), and their solubility was statistically similar (p > 0.05). ABRZ of similar thickness was observed with both adhesives.

CONCLUSION: The new 2-SEA exhibited stable dentin bonding and increased hydrophobicity resulting from the absence of hydrophilic monomers.

PMID:34817966 | DOI:10.3290/j.jad.b2288233

Nov 24 2021

Can a New HEMA-free Two-step Self-etch Adhesive Improve Dentin Bonding Durability and Marginal Adaptation?

J Adhes Dent. 2021 Dec 3;23(6):505-512. doi: 10.3290/j.jad.b2288233.

ABSTRACT

PURPOSE: A new two-step self-etch adhesive (2-SEA) free of hydrophilic monomers was evaluated. Its microtensile bond strength (µTBS) to dentin under various aging conditions, interfacial gap formation, water sorption/solubility, and formation of an acid-base resistant zone (ABRZ) were evaluated and compared with a gold-standard 2-SEA.

MATERIALS AND METHODS: The new 2-SEA G2-Bond Universal (G2; GC) was compared to Clearfil SE Bond 2 (CSE2, Kuraray Noritake). Their µTBS to sound coronal dentin was tested after 1 week, 10,000 thermal cycles (TC), 20,000 TC, 6 months and 1 year. Failure mode was determined using scanning electron microscopy (SEM). Gap formation at the interface of 2-mm deep tapered cavities with an enamel border was observed using swept-source optical coherence tomography after 1 day, 1 week, 10,000 TC, and 20,000 TC. In addition, water sorption and solubility of the bonding agents was measured, and ABRZ formation was evaluated using SEM.

RESULTS: There was no significant difference in µTBS between G2 and CSE2 (p > 0.05), and the aging conditions had no significant effect on µTBS (p > 0.05). In all groups, cohesive failures prevailed (55%-95%). Interfacial gap formation was initially similar for both adhesives (p > 0.05), but G2 exhibited a significantly lower gap formation than CSE2 after TC (p < 0.05). The water sorption of G2 was significantly lower compared to CSE2 (p < 0.05), and their solubility was statistically similar (p > 0.05). ABRZ of similar thickness was observed with both adhesives.

CONCLUSION: The new 2-SEA exhibited stable dentin bonding and increased hydrophobicity resulting from the absence of hydrophilic monomers.

PMID:34817966 | DOI:10.3290/j.jad.b2288233

Nov 24 2021

Can a New HEMA-free Two-step Self-etch Adhesive Improve Dentin Bonding Durability and Marginal Adaptation?

J Adhes Dent. 2021 Dec 3;23(6):505-512. doi: 10.3290/j.jad.b2288233.

ABSTRACT

PURPOSE: A new two-step self-etch adhesive (2-SEA) free of hydrophilic monomers was evaluated. Its microtensile bond strength (µTBS) to dentin under various aging conditions, interfacial gap formation, water sorption/solubility, and formation of an acid-base resistant zone (ABRZ) were evaluated and compared with a gold-standard 2-SEA.

MATERIALS AND METHODS: The new 2-SEA G2-Bond Universal (G2; GC) was compared to Clearfil SE Bond 2 (CSE2, Kuraray Noritake). Their µTBS to sound coronal dentin was tested after 1 week, 10,000 thermal cycles (TC), 20,000 TC, 6 months and 1 year. Failure mode was determined using scanning electron microscopy (SEM). Gap formation at the interface of 2-mm deep tapered cavities with an enamel border was observed using swept-source optical coherence tomography after 1 day, 1 week, 10,000 TC, and 20,000 TC. In addition, water sorption and solubility of the bonding agents was measured, and ABRZ formation was evaluated using SEM.

RESULTS: There was no significant difference in µTBS between G2 and CSE2 (p > 0.05), and the aging conditions had no significant effect on µTBS (p > 0.05). In all groups, cohesive failures prevailed (55%-95%). Interfacial gap formation was initially similar for both adhesives (p > 0.05), but G2 exhibited a significantly lower gap formation than CSE2 after TC (p < 0.05). The water sorption of G2 was significantly lower compared to CSE2 (p < 0.05), and their solubility was statistically similar (p > 0.05). ABRZ of similar thickness was observed with both adhesives.

CONCLUSION: The new 2-SEA exhibited stable dentin bonding and increased hydrophobicity resulting from the absence of hydrophilic monomers.

PMID:34817966 | DOI:10.3290/j.jad.b2288233

Nov 24 2021

Can a New HEMA-free Two-step Self-etch Adhesive Improve Dentin Bonding Durability and Marginal Adaptation?

J Adhes Dent. 2021 Dec 3;23(6):505-512. doi: 10.3290/j.jad.b2288233.

ABSTRACT

PURPOSE: A new two-step self-etch adhesive (2-SEA) free of hydrophilic monomers was evaluated. Its microtensile bond strength (µTBS) to dentin under various aging conditions, interfacial gap formation, water sorption/solubility, and formation of an acid-base resistant zone (ABRZ) were evaluated and compared with a gold-standard 2-SEA.

MATERIALS AND METHODS: The new 2-SEA G2-Bond Universal (G2; GC) was compared to Clearfil SE Bond 2 (CSE2, Kuraray Noritake). Their µTBS to sound coronal dentin was tested after 1 week, 10,000 thermal cycles (TC), 20,000 TC, 6 months and 1 year. Failure mode was determined using scanning electron microscopy (SEM). Gap formation at the interface of 2-mm deep tapered cavities with an enamel border was observed using swept-source optical coherence tomography after 1 day, 1 week, 10,000 TC, and 20,000 TC. In addition, water sorption and solubility of the bonding agents was measured, and ABRZ formation was evaluated using SEM.

RESULTS: There was no significant difference in µTBS between G2 and CSE2 (p > 0.05), and the aging conditions had no significant effect on µTBS (p > 0.05). In all groups, cohesive failures prevailed (55%-95%). Interfacial gap formation was initially similar for both adhesives (p > 0.05), but G2 exhibited a significantly lower gap formation than CSE2 after TC (p < 0.05). The water sorption of G2 was significantly lower compared to CSE2 (p < 0.05), and their solubility was statistically similar (p > 0.05). ABRZ of similar thickness was observed with both adhesives.

CONCLUSION: The new 2-SEA exhibited stable dentin bonding and increased hydrophobicity resulting from the absence of hydrophilic monomers.

PMID:34817966 | DOI:10.3290/j.jad.b2288233

Oct 13 2021

Anti-Demineralization Effects of Dental Adhesive-Composites on Enamel-Root Dentin Junction

Polymers (Basel). 2021 Sep 29;13(19):3327. doi: 10.3390/polym13193327.

ABSTRACT

Oral biofilm reactor (OBR) and pH cycling (pHC) artificial caries model were employed to evaluate the anti-demineralization effects of four composite filling systems on enamel-root dentin junction. Sixty-four enamel-root dentin blocks (6 mm × 6 mm × 2 mm) each with a cylindrical cavity were randomly assigned to the pHC and OBR group, then four subgroups (n = 8) and filled with either the Beautifil II (BEF, SPRG-filler-containing) or Estelite (EST) composite after the adhesive (either Single Bond Universal (SBU) or FL Bond II (FL, SPRG-filler-containing)). The demineralization lesions of filling interface were examined by micro-computerized tomography (μCT) and swept-source-optical coherence tomography (SS-OCT). According to the degree of interface damage, the caries lesions were sorted into four types: Type A and B (no attachment loss); Type C and D (attachment loss). EST/SBU showed the worst demineralization lesion and attachment loss (100% Type D), while BEF/FL exhibited the shallowest lesion depth (p < 0.05, 145 ± 45 μm on enamel, 275 ± 35 μm on root dentin) and no attachment loss (75% Type A and 25% Type B). Using FL adhesive alone does not effectively reduce enamel demineralization. BEF plays a leading role in acid resistance. The combination of BEF and FL showed a cumulative synergistic effect on anti-demineralization.

PMID:34641143 | PMC:PMC8512347 | DOI:10.3390/polym13193327

Oct 13 2021

Anti-Demineralization Effects of Dental Adhesive-Composites on Enamel-Root Dentin Junction

Polymers (Basel). 2021 Sep 29;13(19):3327. doi: 10.3390/polym13193327.

ABSTRACT

Oral biofilm reactor (OBR) and pH cycling (pHC) artificial caries model were employed to evaluate the anti-demineralization effects of four composite filling systems on enamel-root dentin junction. Sixty-four enamel-root dentin blocks (6 mm × 6 mm × 2 mm) each with a cylindrical cavity were randomly assigned to the pHC and OBR group, then four subgroups (n = 8) and filled with either the Beautifil II (BEF, SPRG-filler-containing) or Estelite (EST) composite after the adhesive (either Single Bond Universal (SBU) or FL Bond II (FL, SPRG-filler-containing)). The demineralization lesions of filling interface were examined by micro-computerized tomography (μCT) and swept-source-optical coherence tomography (SS-OCT). According to the degree of interface damage, the caries lesions were sorted into four types: Type A and B (no attachment loss); Type C and D (attachment loss). EST/SBU showed the worst demineralization lesion and attachment loss (100% Type D), while BEF/FL exhibited the shallowest lesion depth (p < 0.05, 145 ± 45 μm on enamel, 275 ± 35 μm on root dentin) and no attachment loss (75% Type A and 25% Type B). Using FL adhesive alone does not effectively reduce enamel demineralization. BEF plays a leading role in acid resistance. The combination of BEF and FL showed a cumulative synergistic effect on anti-demineralization.

PMID:34641143 | PMC:PMC8512347 | DOI:10.3390/polym13193327

Oct 13 2021

Anti-Demineralization Effects of Dental Adhesive-Composites on Enamel-Root Dentin Junction

Polymers (Basel). 2021 Sep 29;13(19):3327. doi: 10.3390/polym13193327.

ABSTRACT

Oral biofilm reactor (OBR) and pH cycling (pHC) artificial caries model were employed to evaluate the anti-demineralization effects of four composite filling systems on enamel-root dentin junction. Sixty-four enamel-root dentin blocks (6 mm × 6 mm × 2 mm) each with a cylindrical cavity were randomly assigned to the pHC and OBR group, then four subgroups (n = 8) and filled with either the Beautifil II (BEF, SPRG-filler-containing) or Estelite (EST) composite after the adhesive (either Single Bond Universal (SBU) or FL Bond II (FL, SPRG-filler-containing)). The demineralization lesions of filling interface were examined by micro-computerized tomography (μCT) and swept-source-optical coherence tomography (SS-OCT). According to the degree of interface damage, the caries lesions were sorted into four types: Type A and B (no attachment loss); Type C and D (attachment loss). EST/SBU showed the worst demineralization lesion and attachment loss (100% Type D), while BEF/FL exhibited the shallowest lesion depth (p < 0.05, 145 ± 45 μm on enamel, 275 ± 35 μm on root dentin) and no attachment loss (75% Type A and 25% Type B). Using FL adhesive alone does not effectively reduce enamel demineralization. BEF plays a leading role in acid resistance. The combination of BEF and FL showed a cumulative synergistic effect on anti-demineralization.

PMID:34641143 | PMC:PMC8512347 | DOI:10.3390/polym13193327