The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites.

. The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites. Dent Mater J. 2020 Aug 25;: Authors: Aung SZ, Takagaki T, Ikeda M, Nozaki K, Burrow MF, Abdou A, Nikaido T, Tagami J Abstract This study aimed to assess the influence of different light curing units …

続きを読む »

8 29 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites.

. The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites. Dent Mater J. 2020 Aug 25;: Authors: Aung SZ, Takagaki T, Ikeda M, Nozaki K, Burrow MF, Abdou A, Nikaido T, Tagami J Abstract This study aimed to assess the influence of different light curing units …

続きを読む »

8 28 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites

Dent Mater J. 2021 Jan 31;40(1):44-51. doi: 10.4012/dmj.2019-353. Epub 2020 Aug 25. ABSTRACT This study aimed to assess the influence of different light curing units (LCUs) on the polymerization of various flowable resin composites. Three LCUs (Optilux 501, Elipar™ DeepCure-L LED and Bluephase®20i) and eight flowable resin composites: MI FIL Flow, Estelite Flow Quick, Estelite …

続きを読む »

8 28 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites

Dent Mater J. 2021 Jan 31;40(1):44-51. doi: 10.4012/dmj.2019-353. Epub 2020 Aug 25. ABSTRACT This study aimed to assess the influence of different light curing units (LCUs) on the polymerization of various flowable resin composites. Three LCUs (Optilux 501, Elipar™ DeepCure-L LED and Bluephase®20i) and eight flowable resin composites: MI FIL Flow, Estelite Flow Quick, Estelite …

続きを読む »

8 28 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites

Dent Mater J. 2021 Jan 31;40(1):44-51. doi: 10.4012/dmj.2019-353. Epub 2020 Aug 25. ABSTRACT This study aimed to assess the influence of different light curing units (LCUs) on the polymerization of various flowable resin composites. Three LCUs (Optilux 501, Elipar™ DeepCure-L LED and Bluephase®20i) and eight flowable resin composites: MI FIL Flow, Estelite Flow Quick, Estelite …

続きを読む »

8 28 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites

Dent Mater J. 2021 Jan 31;40(1):44-51. doi: 10.4012/dmj.2019-353. Epub 2020 Aug 25. ABSTRACT This study aimed to assess the influence of different light curing units (LCUs) on the polymerization of various flowable resin composites. Three LCUs (Optilux 501, Elipar™ DeepCure-L LED and Bluephase®20i) and eight flowable resin composites: MI FIL Flow, Estelite Flow Quick, Estelite …

続きを読む »

8 28 2020

The effect of different light curing units on Vickers microhardness and degree of conversion of flowable resin composites

Dent Mater J. 2021 Jan 31;40(1):44-51. doi: 10.4012/dmj.2019-353. Epub 2020 Aug 25. ABSTRACT This study aimed to assess the influence of different light curing units (LCUs) on the polymerization of various flowable resin composites. Three LCUs (Optilux 501, Elipar™ DeepCure-L LED and Bluephase®20i) and eight flowable resin composites: MI FIL Flow, Estelite Flow Quick, Estelite …

続きを読む »

古い記事へ «